Nanoindentation (single cycle) test data for Gr. 91 material at 23 °C and maximum indenter force of 100.13028 mN

Open data API in a single place

Provided by Joint Research Centre

Get early access to Nanoindentation (single cycle) test data for Gr. 91 material at 23 °C and maximum indenter force of 100.13028 mN API!

Let us know and we will figure it out for you.

Dataset information

Country of origin
Updated
2018.03.16 00:00
Created
Available languages
English
Keywords
Engineering material properties
Quality scoring
290

Dataset description

Data created at the European Commission JRC in the scope of the EERA JPNM pilot project NINA on the topic of nanoindentation for nuclear applications.
Build on reliable and scalable technology
Revolgy LogoAmazon Web Services LogoGoogle Cloud Logo
FAQ

Frequently Asked Questions

Some basic informations about API Store ®.

Operation and development of APIs are currently fully funded by company Apitalks and its usage is for free.
Yes, you can.
All important information such as time of last update, license and other information are in response of each API call.
In case of major update that would not be compatible with previous version of API, we keep for 30 days both versions so you will have enough time to transfer to new version. We will inform you about the changes in advance by e-mail.

Didn't find the API you need?

Let us know and we will figure it out for you.

API Store provides access to European Open Data via scalable and reliable REST API interface.
Copyright © 2026. Made with ♥ by Apitalks