Small punch creep test data for 2.25 Cr 1Mo V mod material at 600 °C and a load of 230 N

Open data API in a single place

Provided by Joint Research Centre

Get early access to Small punch creep test data for 2.25 Cr 1Mo V mod material at 600 °C and a load of 230 N API!

Let us know and we will figure it out for you.

Dataset information

Country of origin
Updated
2016.02.26 00:00
Created
Available languages
English
Keywords
Elevated temperature material properties
Quality scoring
290

Dataset description

Data collection created in the scope of a programme designed to evaluate the reliability of the Small Punch (SP) testing method as an alternative mechanical test technique for evaluation of the residual life and integrity assessment of components in ageing plants. Tests were performed on the low alloy - 2¼Cr 1Mo V modified ferritic steel, widely selected for construction of high temperature components in petrochemical plants. The technique was shown to facilitate determination of both creep and tensile properties of materials. However, special attention was directed to the potential of the SP creep testing technique for assessing the deterioration of material due to hydrogen attack and thermal ageing, in comparison with conventional uniaxial creep methods.
Build on reliable and scalable technology
Revolgy LogoAmazon Web Services LogoGoogle Cloud Logo
FAQ

Frequently Asked Questions

Some basic informations about API Store ®.

Operation and development of APIs are currently fully funded by company Apitalks and its usage is for free.
Yes, you can.
All important information such as time of last update, license and other information are in response of each API call.
In case of major update that would not be compatible with previous version of API, we keep for 30 days both versions so you will have enough time to transfer to new version. We will inform you about the changes in advance by e-mail.

Didn't find the API you need?

Let us know and we will figure it out for you.

API Store provides access to European Open Data via scalable and reliable REST API interface.
Copyright © 2026. Made with ♥ by Apitalks