Small punch creep test data for P91 material at 600 °C and a load of 314 N (third repeat test)

Open data API in a single place

Provided by Joint Research Centre

Get early access to Small punch creep test data for P91 material at 600 °C and a load of 314 N (third repeat test) API!

Let us know and we will figure it out for you.

Dataset information

Country of origin
Updated
2017.08.02 00:00
Created
Available languages
English
Keywords
Elevated temperature material properties
Quality scoring
290

Dataset description

Data produced during work to evaluate the creep and fracture properties of P91 steel by small punch testing. The tests were performed on material extracted from the same pipe used in the INTEGRITY FP5 Growth Project (GRD 1/10886. 2005.), the data for which are also hosted at the JRC Petten ODIN portal.
Build on reliable and scalable technology
Revolgy LogoAmazon Web Services LogoGoogle Cloud Logo
FAQ

Frequently Asked Questions

Some basic informations about API Store ®.

Operation and development of APIs are currently fully funded by company Apitalks and its usage is for free.
Yes, you can.
All important information such as time of last update, license and other information are in response of each API call.
In case of major update that would not be compatible with previous version of API, we keep for 30 days both versions so you will have enough time to transfer to new version. We will inform you about the changes in advance by e-mail.

Didn't find the API you need?

Let us know and we will figure it out for you.

API Store provides access to European Open Data via scalable and reliable REST API interface.
Copyright © 2026. Made with ♥ by Apitalks